Anatomical, physical-mechanicalandmachiningcharacteristics of the wood of velvet mesquite (Prosopis velutina Wooton)

Authors

  • Raúl Rodríguez Anda Departamento de Madera, Celulosa y Papel. Universidad de Guadalajara
  • Alejandra María Ramírez Arango Posgrado del Departamento de Madera, Celulosa y Papel. Universidad de Guadalajara
  • Hilda Palacios Juárez Departamento de Madera, Celulosa y Papel. Universidad de Guadalajara
  • Francisco Javier Fuentes Talavera Departamento de Madera, Celulosa y Papel. Universidad de Guadalajara
  • José Antonio Silva Guzmán Departamento de Madera, Celulosa y Papel. Universidad de Guadalajara
  • Alma Rosa Saucedo Corona Departamento de Madera, Celulosa y Papel. Universidad de Guadalajara

DOI:

https://doi.org/10.29298/rmcf.v6i28.257

Keywords:

Wood anatomy, dimensional stability, machining of the wood, mechanical properties, Prosopis velutina Wooton, wood resistance

Abstract

The anatomical, physical-mechanical and machining characteristics of the wood of velvet mezquite (Prosopis velutina) were determined. Five two-meter logs were collected from stumps in the state of Sonora. The anatomical study was carried out in compliance with IAWA. The physical-mechanical properties were evaluated according to the DIN standards. The machining was done manually, and the surface was evaluated according to the norm ASTM D 1666-87. The wood was found to have a diffuse to semi-annular porosity. Heartwood with abundant amber-colored deposits in the vessels and in the axial and radial parenchyma. Average length and thickness of the fibers of 863 μm and 4.3 μm, respectively. Paratracheal winged-aliform parenchyma. Homocellular core radii. Prismatic crystals abound in the chambered axial parenchyma. The basic density of the timber is very high (0.79 g cm-3) and its dimensional stability is good. Resistance to flexion was classified as medium (17 N mm-2), and the modulus of elasticity, as low (1 232 N mm-2). Resistance to longitudinal compression was classified as very high (87 N mm-2), and the modulus of elasticity, as low (1 915 N mm-2). Resistance to impact is rated fair (51 kJ m-2). In the presence of shearing, it is considered to be hard (19 N mm-2). Its Brinell hardness is rated very high (72 N mm-2 tangential; 73 N mm-2 radial and 96 N mm-2 longitudinal). Its response to gluing is considered to be good (Leve l 5; 7 N mm-2). Its machining is classified as good, and therefore cutting tools with tungsten carbide valve seats are required.

Downloads

Download data is not yet available.

Downloads

Published

2018-03-21

Issue

Section

Scientific article

How to Cite

Rodríguez Anda Raúl, Ramírez Arango Alejandra María, Palacios Juárez Hilda, Francisco Javier Fuentes Talavera, Silva Guzmán José Antonio, and Alma Rosa Saucedo Corona. 2018. “Anatomical, Physical-Mechanicalandmachiningcharacteristics of the Wood of Velvet Mesquite (Prosopis Velutina Wooton)”. Revista Mexicana de Ciencias Forestales 6 (28): 156-73. https://doi.org/10.29298/rmcf.v6i28.257.